Publication:
Optimizing of the cementitious composite matrix by addition of steel wool fibers (Chopped) based on physical and mechanical analysis

cris.virtual.department Universiti Malaysia Perlis
cris.virtual.department Universiti Malaysia Perlis
cris.virtual.department Universiti Malaysia Perlis
cris.virtualsource.department 1fb76e68-0c75-4529-ac9f-cf51941493f8
cris.virtualsource.department 9414f569-850d-45d8-8fa2-e5f2c4194711
cris.virtualsource.department 4ef9a0c1-06ba-415b-a708-a0f9148b37ff
dc.contributor.author Akrm A Rmdan Amer
dc.contributor.author Mohd. Mustafa Al Bakri Abdullah
dc.contributor.author Liew Yun Ming
dc.contributor.author Jerzy J. Wysłocki
dc.contributor.author Wojciech Sochacki
dc.contributor.author Ikmal Hakem A Aziz
dc.contributor.author Muhammad Faheem Mohd. Tahir
dc.contributor.author Sebastian Garus
dc.contributor.author Joanna Gondro
dc.contributor.author Hetham A. R. Amer
dc.date.accessioned 2024-04-04T04:59:58Z
dc.date.available 2024-04-04T04:59:58Z
dc.date.issued 2021
dc.description.abstract The demand for durable, resistant, and high-strength structural material has led to the use of fibers as reinforcing elements. This paper presents an investigation into the inclusion of chopped steel wool fibers (CSWFs) in cement to form a high-flexural strength cementitious composite matrix (CCM). CSWFs were used as the primary reinforcement in CCM at increments of 0.5 wt%, from 0.5–6 wt%, with ratios of cement to sand of 1:1.5 and water to cement of 0.45. The inclusion of CSWFs resulted in an excellent optimization of the physicomechanical properties of the CCM, such as its density (2.302 g/cm3), compressive strength (61.452 MPa), and maximum flexural strength (10.64 MPa), all of which exceeded the performances of other reinforcement elements reported in the literature.
dc.identifier.doi 10.3390/ma14051094
dc.identifier.uri https://www.mdpi.com/1996-1944/14/5/1094
dc.identifier.uri https://www.mdpi.com/journal/materials
dc.identifier.uri https://hdl.handle.net/20.500.14170/2031
dc.language.iso en
dc.relation.ispartof Materials
dc.relation.issn 1996-1944
dc.subject Steel Wool Fiber
dc.subject Chopped Fiber
dc.subject Cement Composite
dc.title Optimizing of the cementitious composite matrix by addition of steel wool fibers (Chopped) based on physical and mechanical analysis
dc.type journal-article
dspace.entity.type Publication
oaire.citation.endPage 14
oaire.citation.issue 5
oaire.citation.startPage 1
oaire.citation.volume 14
oairecerif.author.affiliation Universiti Malaysia Perlis
oairecerif.author.affiliation Universiti Malaysia Perlis
oairecerif.author.affiliation Universiti Malaysia Perlis
oairecerif.author.affiliation Czestochowa University of Technology, Poland
oairecerif.author.affiliation #PLACEHOLDER_PARENT_METADATA_VALUE#
oairecerif.author.affiliation Universiti Malaysia Perlis
oairecerif.author.affiliation Universiti Malaysia Perlis
oairecerif.author.affiliation Czestochowa University of Technology, Poland
oairecerif.author.affiliation Czestochowa University of Technology, Poland
oairecerif.author.affiliation Omar Al Mukhtar Universiti
Files
Original bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
Optimizing of the Cementitious Composite Matrix (D).pdf
Size:
6.39 MB
Format:
Adobe Portable Document Format
Description:
Collections