Home
  • English
  • Čeština
  • Deutsch
  • Español
  • Français
  • Gàidhlig
  • Latviešu
  • Magyar
  • Nederlands
  • Português
  • Português do Brasil
  • Suomi
  • Log In
    New user? Click here to register. Have you forgotten your password?
Home
  • Browse Our Collections
  • Publications
  • Researchers
  • Research Data
  • Institutions
  • Statistics
    • English
    • Čeština
    • Deutsch
    • Español
    • Français
    • Gàidhlig
    • Latviešu
    • Magyar
    • Nederlands
    • Português
    • Português do Brasil
    • Suomi
    • Log In
      New user? Click here to register. Have you forgotten your password?
  1. Home
  2. Resources
  3. UniMAP Index Publications
  4. Publications 2022
  5. In vitro biodegradation, cytotoxicity, and biocompatibility of polylactic acid/napier cellulose nanofiber scaffold composites
 
Options

In vitro biodegradation, cytotoxicity, and biocompatibility of polylactic acid/napier cellulose nanofiber scaffold composites

Journal
International Journal of Biological Macromolecules
ISSN
01418130
Date Issued
2022-12-31
Author(s)
Revati R.
Mohd Shukry Abdul Majid
Universiti Malaysia Perlis
Mohd Ridzuan Mohd Jamir
Universiti Malaysia Perlis
Normahira Mamat @ Mohamad Nor
Universiti Malaysia Perlis
Cheng Ee Meng
Universiti Malaysia Perlis
Alshahrani H.A.
DOI
10.1016/j.ijbiomac.2022.11.041
Handle (URI)
https://hdl.handle.net/20.500.14170/9145
Abstract
This study aimed to evaluate the bioactivities and biocompatibilities of porous polylactic acid (PLA) reinforced with cellulose nanofiber (CNF) scaffolds. The in vitro degradation behaviors of the porous PLA/CNF scaffolds were systematically measured for up to 8 weeks in a phosphate-buffered saline medium at 37 °C. The reinforcement of CNF resisted the biodegradation of the scaffolds. The in vitro cytotoxicity and biocompatibility of the scaffolds were determined using the Beas2B American Type Culture Collection cells. The 3-(4,5-cimethylthiazol-2-yl)-2,5-diphenyl tetrazolium bromide cytotoxicity and proliferation tests showed that the scaffolds were non-toxic, and epithelial cells grew well on the scaffold after 7 days of culture, whereas the percentage of cell proliferation on the PLA/CNF15 scaffold was the largest, 130 %. A scratch wound-healing assay was performed to evaluate the suitability of the scaffolds for cell migration. The results demonstrated that the scaffolds exhibited good cell migration towards nearly complete wound closure.
Funding(s)
Ministry of Higher Education, Malaysia
Subjects
  • Cell proliferation | ...

File(s)
Research repository notification.pdf (4.4 MB)
Downloads
18
Last Month
1
Acquisition Date
Oct 15, 2025
View Details
Views
2
Last Week
1
Last Month
1
Acquisition Date
Oct 15, 2025
View Details
google-scholar
  • About Us
  • Contact Us
  • Policies