Now showing 1 - 2 of 2
  • Publication
    The Effect of NaOH Concentration on Palm Oil Boiler Ash (POBA) based Geopolymer Artificial Aggregate
    Industrial wastes or by-products can be used to create artificial aggregates. Solid waste created by the palm oil industry is a significant environmental problem that requires immediate and long-term solutions. The optimal ratio of geopolymer-based palm oil boiler ash (POBA) aggregate in terms of specific gravity, water absorption, and aggregate impact value was explored in this work. Because of its high percentages of silica oxide (SiO2) and aluminium oxide (Al2O3), POBA was chosen as the primary precursor for the geopolymer (Al2O3). The POBA aggregate with the lowest specific gravity was 1.662, while all of the geopolymer-based POBA aggregates had specific gravities below 2. The geopolymer-based POBA aggregate absorbs more water than the natural aggregate. The aggregate effect value for sodium hydroxide concentrations (6M, 8M, 10M, 12M, 14M) is less than 30%, which is considered strong.
      1
  • Publication
    The ProPerTies of Ground GranulaTed BlasT furnace slaG liGhTweiGhT aGGreGaTe (Gla) aT Various Molar raTio and iTs aPPlicaTion in concreTe
    ( 2023-01-01) ;
    Hassan M.A.
    ;
    ; ;
    Ariffin M.A.M.
    ;
    ;
    Hao D.L.C.
    The effects of supplementary cementitious materials (SCM) on the characteristics and internal structure of synthetic aggregate made from ground granulated blast furnace slag are investigated in this study (GGBS). Due to its high pozzolanic activity, GGBS was shown to be superior to other SCM materials, enhancing both the strength and durability of synthetic aggregate. Because sintering uses a lot of energy and generates a lot of pollutants, using a cold-bonded approach to make low density lightweight aggregates is particularly significant from an economic and environmental standpoint. Thus, the utilisation of ground granulated blast furnace slag (GGBS) as a substitute material in the production of green artificial lightweight aggregate (GLA) using the cold bonding method was discussed in this work. Admixtures of ADVA Cast 203 and Hydrogen Peroxide were utilised to improve the quality of GLA at various molar ratios. The freshly extracted GLA was then evaluated for specific gravity, water absorption, aggregate impact, and aggregate crushing in order to determine the optimal proportion blend. As a result, the overall findings offer great application potential in the development of concrete (GCLA). It has been determined that aggregates with a toughness of 14.6% and a hardness of 15.9% are robust. The compressive strength test found that the GCLA has a high strength lightweight concrete of 37.19 MPa and a density of 1845.74 kg/m3. The porous features developed inside the internal structure of GLA have led to GCLA’s less weight compared to conventional concrete.
      2